The Influence of Technological and Tribological Factors on the Aftereffect and Wear Resistance of Polymer Composites

Authors

  • H.O. Sirenko Vasyl Stefanyk Precarpathian National University
  • A.V. Lutsas Vasyl Stefanyk Prekarpathian University
  • M.B. Skladanyuk Vasyl Stefanyk Prekarpathian University
  • L.M. Soltys Vasyl Stefanyk Prekarpathian University

DOI:

https://doi.org/10.15330/pcss.16.2.360-372

Keywords:

carbon fibers, polymer composites, anti-wear properties, friction, wear, aftereffect

Abstract

The anti-wear properties of polymer composites based on polytetrafluoroethylene with not metallized and metallized carbon fibers in conditions of friction and wear in over limit and limit of specific loads have been researched. The definitions of loading and time indicators the aftereffect which give the quantitative assessment of influence processes and mechanism of friction and wear have been introduced first. It is established that in anti-wear tests of composites samples as in stepped over limit specific load (Ni=var) as in constant limit and specific load (Ni=const) with high probability appears time aftereffect.

References

[1] G. O. Sіrenko, Stvorennja antifrikcіjnih materіalіv na osnovі poroshkіv termotrivkih polіmerіv ta vuglecevih volokon: Dis. … dokt. tehn. nauk (Іn-t problem materіaloznavstva іm. І.M. Francevicha NANU, Kiїv, 1997).
[2] A.s. 1604862 (USSR), MKI S23S18/38; S23S18/54/ (1990).
[3] A.s. 1736171 (USSR), MKI C08J5/16; C08L27/18/ (1992).
[4] A.s. 1723084 (USSR), MKI C08J5/16; C08L27/18/ (1992).
[5] A.s. 110292 (USSR), MKI S08J5/16; S08L27/18/ (1977).
[6] A.s. 181484 (USSR), MKI F16C33/12/ (1982).
[7] A.s. 1078907 (USSR), MKI S08L27/18; S 08J5/16/ (1984).
[8] A.s. 194601 (USSR), MKI F16C33/12/ (1983).
[9] A.s. 1239134 (USSR), MKI S08J5/16; S08J5/06/ (1986).
[10] A.s. 1165048 (USSR), MKI S08L27/18; S08K3/04/ (1985).
[11] A.s. 1244933 (USSR), MKI S08J5/16; S08L27/18/ (1986).
[12] A.s. 223896 (USSR), MKI S08L77/10/ (1985).
[13] A.s. 1635523 (USSR), MKI C08J5/16; C08L27/18/ (1990).
[14] A.s. 1584365 (USSR), MKI S08L77/10/ (1990).
[15] P.r. №4539382/05/01619 (1992).
[16] Pat. 1806147 (USSR), MKI S08J9/26; B01D39/16/ (1993).
[17] A.s. 1590778 (USSR), MKI F16J15/20/(1990).
[18] A.s. 1587300 (USSR), MKI F16J15/00; F16J15/22/ (1990).
[19] A.s. 1545584 (USSR), MKI S08L77/02; S08K13/02/ (1990).
[20] A.s. 1467893 (USSR), MKI V32V3/12; D04S5/00; F16C33/12/(1989).
[21] A.s. 1460492 (USSR), MKI F16J15/00/ (1989).
[22] A.s. 1400040 (USSR), MKI S08J5/16; S08L77/08/ (1988).
[23] A.s. 1322664 (USSR), MKI S08L77/10/ (1987).
[24] A.s. 558518 (USSR), MKI S08L77/06/ (1977).
[25] A.s. 526252 (USSR), MKI S08L77/00; S08D5/16/ (1976).
[26] G. O. Sіrenko, M. B. Kvich, V. І. Kirichenko, Fіzika і hіmіja tverdogo tіla, 7 (3), 544 (2006).
[27] G. O. Sіrenko, M. B. Kvich, V. І. Kirichenko, Vіsnik Prikarp. nac. un-tu іm. V.Stefanika. Ser. Hіmіja, V, 84 (2008).
[28] V. I. Kirichenko, G. A. Sirenko, L. M. Kirichenko, Voprosy himii i himicheskoj tehnologii, 94, 113 (1991).
[29] G. O. Sіrenko, L. M. Soltis, V. І. Kirichenko, V. P. Svіders'kij, M. B. Skladanjuk, Vіsnik Prikarp. nac. un-tu іm. Vasilja Stefanika. Ser.Hіmіja, HIV, 50 (2012).
[30] G. O. Sіrenko, M. B. Skladanjuk, L. M. Soltis, Fіzika і hіmіja tverdogo tіla, 16 (1) (2015).
[31] G. O. Sіrenko, O. V. Shijchuk, Kompozicіjnі polіmernі materіali, 25 (1), 49 (2003).
[32] A. V. Gorjaninova, G. K. Bozhkov, M. S. Tihonova, Ftoroplasty v mashinostroenii (Mashinostroenie, Moskva, 1971).
[33] D. D. Chegodaev, Z. K. Naumova, C. S. Dunaevskaja, Ftoroplasty (Goshimizdat, Leningrad, 1960).
[34] D. Mur, Osnovy i primenenie triboniki (Mashinostroenie, Moskva, 1968).

Published

2015-06-15

How to Cite

Sirenko, H., Lutsas, A., Skladanyuk, M., & Soltys, L. (2015). The Influence of Technological and Tribological Factors on the Aftereffect and Wear Resistance of Polymer Composites. Physics and Chemistry of Solid State, 16(2), 360–372. https://doi.org/10.15330/pcss.16.2.360-372

Issue

Section

Scientific articles

Most read articles by the same author(s)

1 2 > >>